Hi

I have a red Trichord (Corso style).

The Screw on celluloid on keyboard face is slightly curved. Nothing major, flat in the area of the buttons but curves gently down as it goes under the metal grill – just enough so that the grill can be pushed over the top of the small strip of plastic attached to the keyboard face for the purpose of preventing the grill being pushed in.

I understand that celluloid is a thermoplastic and am used to shaping/reshaping acrylic (also a thermoplastic) with ovens and strip heaters, but I can’t really afford to go about this through a trial and error processes. So any tips/advice welcome.

I do note that the keyboard face does not appear to be a single thick piece of celluloid - looks like 3 layers (thin –thick –thin)  Is the darker coloured middle layer also celluloid?

Thanks

Andy 
Title: Re: Celluloid question
Post by: Theo on September 22, 2013, 04:09:50 PM
Yes usually all layers are celluloid.  I think the safest method of heating celluloid (to avoid fire risk) is in a water bath.
Title: Re: Celluloid question
Post by: Nick Collis Bird on September 22, 2013, 04:12:14 PM
Yes usually all layers are celluloid.  I think the safest method of heating celluloid (to avoid fire risk) is in a water bath.
Concur, 8)
Title: Re: Celluloid question
Post by: Kimric Smythe on September 23, 2013, 05:31:48 AM
I have had good luck with a hair dryer set on high. set the part you are working on on a smooth flat surface like wood or cardstock with a firm backing like a table top. you will want a smooth piece of wood to use to press it flat as you heat it.