Title: Flattening Pearloid.
Post by: Henry Piper on September 23, 2021, 11:17:18 AM
Does anyone have a suggestions for flattening pearloid.  I have a very nice pierced grille from an Italian P.A that I wish to re-purpose for use on a pearloid covered Hohner pokerwork style box ?  This grille is quite severely dished, and as it is presumably Celluloid based, I am looking for a safe and reliable method of flattening it.
Title: Re: Flattening Pearloid.
Post by: Gav Wood on September 25, 2021, 07:58:41 AM
Will tell you my experiences if it helps you decide what not to do…

A whole box side i melted too much and went through some of the top coat before i got it stuck back in place, this one the perloid layer was clear, and the colour underneath, you could split the 2 layers apart. I practiced first but the piece was a lot smaller and the large piece had more weight so stretched too far before i got it back on.

A bend the length of the box from straight worked out ok on a hohner though, that was a piano to button conversion, cut the backing material off, bent the back of the fingerboard round.into quite a tight  bend, then reset, no chemical needed.

If it is a dish rather than a bow, i think you may split it unless you use acetone water mix to soften the celluloid, i have had material split where trying to bend where it would not compress and i had not softened it.

If there is spare material on the donor box, i would experiment with that first, have had success with plastics and heat, boiling water works for some, but others need the acetone and water mix bath.

All my perloid grilles are mounted on aluminium, where i have straightened in the the past, they have been fine manually bending them.
Title: Re: Flattening Pearloid.
Post by: Rog on September 25, 2021, 03:40:07 PM
I’d try heating it with a hair dryer and straightening it out when pliable. Else if it’s mounted on metal just bend the metal straight.
Title: Re: Flattening Pearloid.
Post by: Tone Dumb Greg on September 25, 2021, 05:04:59 PM
Would a hot wire bender (as used for acrylic) work. They cost a ridiculous amount ready made, but you can make a DIY one very cheaply.

https://www.youtube.com/watch?v=YUKabFvPbIU
Title: Re: Flattening Pearloid.
Post by: Theo on September 25, 2021, 05:10:47 PM
I've not tried this, but I think immersing in hot water will be the safest method.   Even heating guaranteed, and you can easily try a moderate temperature, then gradually increase it as required.  You need some kind of fixture to hold it in the correct shape while it cools.
Title: Re: Flattening Pearloid.
Post by: Tone Dumb Greg on September 25, 2021, 05:19:20 PM
Would a hot wire bender (as used for acrylic) work. They cost a ridiculous amount ready made, but you can make a DIY one very cheaply.

https://www.youtube.com/watch?v=YUKabFvPbIU

I've just realised that my idea wouldn't work because more than one fold is required...unless??? I've just thought of a way round that. It would need reasonable temperature regulation, though.

If it softens below 100 degrees C Theo's method is, clearly, best.
Title: Re: Flattening Pearloid.
Post by: Kimric Smythe on October 01, 2021, 05:18:36 PM
I use a heat gun and blocks of wood to flatten and shape the celluloid. if you are getting a strong camphor smell you are getting it too hot.
It cools very fast and is kinda slow to heat up, it has very little thermal mass.
Title: Re: Flattening Pearloid.
Post by: Henry Piper on October 02, 2021, 02:02:16 PM
Thanks everyone for your suggestions,..... Application of Hot water and heavy weight seems to have done the trick !!!