I know some people think they are naff, but I like chrome grills. My new Loffet Pro and Club IV (a wonderful Theo restoration) Gleem beautifully, but the G/D Club Victoria (another Theo masterpiece) and The Lilliput are decidely tarnished.
Can they be re-chromed, or in any way brought up to full gleeming glory. Alternatively would it be possible to make new grills with distinctive designs?
On the same theme, is there anything that will put a real shine back into perloid that's gone a bit dull?
Just cosmetic I know, but sometimes late at night when playing is out of the question, I like to get the boxes out and just look at them. Works of art every one of them.
-
Don't know for sure, but I've always assumed that the grille is made of brass if it's chromed. The old way was to flash nickel plate the brass and then chrome it for best results of adhesion and eveness of plating. I would guess that the nickel flash would be too expensive for things like a grille. Try scratching the inside of the grille to see if it is brass, in which case it could be polished and rechromed.
Alternatively, a new grille could be fashioned from any available metal if you have the skill and patience to do the decorative piercing. Aluminium could be anodised in a choice of colours or brass could be chromed.
The current trend with Italian built designs seems to be to make a pierced aluminium grille and then veneer it with wood matching the box. This allows folds and curves that the wood would not otherwise tolerate.
Rob.
-
There are plenty of chroming companies who service the classic car people for example;
http://www.londonchroming.co.uk/ (http://www.londonchroming.co.uk/)
-
The homebrew way of doing it is to make sure that the grille is scrupulously clean by giving it a good rub with wire wood, making sure you get any rusty dust off it, and then using a silver spray enamel. Give it a really thin coat (probably wont cover it all) and leave to dry. You can then do 2,3 or 4 coats to give it a really good covering, leaving to dry each time. You'll never get the shine or texture of a chromed grille, but it does provide a good low cost solution and the enamel gives the metal a protective layer to stop further rusting.
-
On the same theme, is there anything that will put a real shine back into perloid that's gone a bit dull?
Nick
Do a search for "celluloid polishing" there's a whole thread on this.
Simon
-
are you shure that really chrome was used ? ... The melodeon, which I'm currently restoring,
seems to have tinned metal plates (as seen on this image : http://www.myimg.de/?img=schwirsch103601.jpg )
-
Michael, that looks to me like nickel plating.
Don't know for sure, but I've always assumed that the grille is made of brass if it's chromed. The old way was to flash nickel plate the brass and then chrome it for best results of adhesion and eveness of plating. I would guess that the nickel flash would be too expensive for things like a grille. Try scratching the inside of the grille to see if it is brass, in which case it could be polished and rechromed.
I don't see why nickel would make it too expensive? Decent chrome plate always has nickel plate underneath it, and sometimes copper under that. They can also be applied to steel.
The key to a good plating job is that the base metal must be polished first and must be very clean. Any scratches, rust pits roughness etc will still show after the plating has been applied.
-
Michael, that looks to me like nickel plating.
Are there some specific tests to find out, what it is actually ?
In my case the coating is only on one side
Michael
-
Its just the colour. Chrome has a very slightly bluish colour, nickel is a warmer colour, with a hint of yellow.
It doesn't really matter, because if you take it to a plating shop they will be able to tell straight away.
-
I only suggested that double plating might be too expensive as it is one more process, not inherently expensive. Plating on steel used to be done as Theo says with copper/nickel/chrome and polished before each stage. The smartest motorbike I ever saw had a black chromed frame left unpolished, giving a semi-matt sheen - fantastic!
Rob.
-
Plating is done in a succession of dip baths so a nickel strike matters not. at least it makes sure the chrome adheres.