Melodeon.net Forums
Discussions => Instrument Design, Construction and Repair => Topic started by: Rog on April 09, 2017, 07:42:10 AM
-
I've had a look through the threads....but still have this question.
Once a celluloid repair has been made e.g. Patching a thumbnail sized hole on a corner of a Corona, the celluloid can be evened out with glass paper. But what is the technique for getting a glassy smooth surface? How do you convert a matt finish to a polished finish?
-
There are more experts here than me Rog
But I would try jewellers rouge with a Dremel buffing pad. Now come on! You have got a Dremel,haven't you? >:E
-
Hi Roger,
Firstly,dont use glass or sandpaper,use very fine wet and dry on a cork block to level ,use circular motion and very gently.
If on a corner fold paper three times to make thicker and hold rather than on block
Then use fercell G3 then G10 to finish.,
Pete
-
Hi both, thanks. Yes I have a Dremel and buffing compound. Just thought I'd ask. I have a busted Corona end to practice on (:) before I repair the replacement.
-
Hi both, thanks. Yes I have a Dremel and buffing compound. Just thought I'd ask. I have a busted Corona end to practice on (:) before I repair the replacement.
Very easy to good too fast with a Dremel and burn the celluloid
-
Brasso or other metal polish works well. Apply by hand on a soft cloth.
-
Yes I agree with Theo, Brasso is the best way to get a good finish on plastics of all sorts. I have also had good results with a red powder which was what we used to polish spectacle lenses many years ago, when I worked in that trade. The trade name was Serirouge, or Cerirouge, but I assume it's a variation of jeweler's rouge. The best thing I have found for a final polish, is Mer polish.
Hand polishing works best, power tools are too fast, and over enthusiastic use, can melt the surface of most plastics.
Sir John
-
Hi both, thanks. Yes I have a Dremel and buffing compound. Just thought I'd ask. I have a busted Corona end to practice on (:) before I repair the replacement.
Very easy to good too fast with a Dremel and burn the celluloid
Hmmm! I use a Dremel to polish Abalone and other shells to a really high finish. It depends on how hard you push. You would have to be very heavy handed to spoil celluloid.
-
Does Brasso contain a v fine abrasive? I use stuff called Safe Cut, which is a less aggressive version of T Cut, when cleaning up boxes. But in the case of matt celluloid it needs to bring up a shine. I'll give Brasso a go too.
-
Very easy to good too fast with a Dremel and burn the celluloid
[/quote]
Hmmm! I use a Dremel to polish Abalone and other shells to a really high finish. It depends on how hard you push. You would have to be very heavy handed to spoil celluloid.
[/quote]
You only have to be slightly heavy handed to damage celluloid using a powered buffing mop. It softens with only a slight increase in temperature, then the buff starts to catch the softened surface and very quickly you have a ploughed field!
-
That sounds like the voice of experience. Thanks Theo. I now have this image of you happily buffing some celluloid with a drill mop and suddenly 'oh <expletive>'...
-
That's about it. Nothing quite like learning from mistakes.
-
That's about it. Nothing quite like learning from mistakes.
Learning from other's mistakes is better though (:)
-
;D
-
Hi Roger,
Firstly,dont use glass or sandpaper,use very fine wet and dry on a cork block to level ,use circular motion and very gently.
If on a corner fold paper three times to make thicker and hold rather than on block
Then use fercell G3 then G10 to finish.,
Pete
Pete...what is the fercell stuff you mention?
-
Maybe this. (http://www.farecla.com/automotive/compounding-systems/advanced-g3-liquid-compound)
-
That's the stuff,
I them finish with autoglym car polish because it has a very slight abrasive action
-
Tooth paste works quite well too!
-
That's what I use on my windscreen, to clear oily greasy film. It works well.
Sir John
-
Tooth powder also. Preferably smokers, but you won't get the high polish that brasso gives.
-
I use the same stuff car people use to polish paint. There are large ,fine and haze removing compounds that I use in the shop all the time. These can be found at any car parts shop. The final polish compound works great on aluminum trim too.
-
I've used T Cut with good effect on celluloid and keep polishing until the cloth shows no more dirt. A coat of Canuba wax on top makes a good finish. Go gently over transfers. I've found that a gentle wipe over improves the look of those too.
-
There are compounds formulated to remove oxidation from vinyl boat windows which I have used successfully. Rubbing compound is one name for the material used to polish automotive lacquer. Cerium oxide is another option which I use to bring glass to a highly polished finish after grinding to desired shape.
-
to polish celluloid I have used a kit to polish the headlights of cars, these usually become yellowish and grated after a long time. The kit in question has 4 numbered pads, are actually sandpaper but incredibly thin a white polishing paste and a specific liquid for the finish. I did not use the final liquid.
First the thicker one is used and the fine one (it is not no mystery) is finished and then the white paste with cotton is passed.
The result is very good and less dangerous, with the dremel you have to be very tactful and do not push too much because it burns.
The product is called Turtle Wax Lens restorer.
-
Brasso or other metal polish works well. Apply by hand on a soft cloth.
I tried this just recently with Brasso. Very lightly by hand and the cloth turned red. Immediately stopped as not wanting to damage the celluloid. Normal for the cloth to pick up the red celluloid with Brasso and furniture polish?
-
I use brasso too, yes the cloth will show some colour because it is a very fine abrasive. Celluloid faces with exposure to light and air and an abrasive polish removes a very fine surface layer which can reveal unfaded material with a brighter colour. It’s exactly the same principle as a cutting polish on car finish.
-
do not......I repeat......DO NOT use eyeglasses cleaning fluid!! 8)
-
"It’s exactly the same principle as a cutting polish on car finish."
In the "olden days" I had a car spray painter who would polish the finished cellulose paint with either Brasso or Mepo (same thing) until a polishing cloth would slide off the bonnet by itself. They are ideal for a very fine finish.
-
Then there's luthier's burnishing cream, if you want to go all posh.
A word from the wise, though. Avoid anything with beeswax, or the like, in it unless you want the box to keep slipping away as you try to play it.
-
I don't think I'd be that keen on polishing unless maybe I wanted to sell the box, and even then it might make me feel guilty - after all, one is wearing away a layer of the celluloid when using an abrasive polish, no matter how carefully.
-
Isn't the lettering screen printed on?
You wouldn't want to polish that off.
-
I don't think I'd be that keen on polishing unless maybe I wanted to sell the box, and even then it might make me feel guilty - after all, one is wearing away a layer of the celluloid when using an abrasive polish, no matter how carefully.
Agreed, polishing with a cutting polish is something to do very occasionally. For regular cleaning a soft cloth dampened with a mild detergent solution is all you need.
-
My celluloid cleaning weapon of choice is T-Cut. It brings up celluloid beautifully...car paint restorer.
Interesting side note: Will on The Repair Shop uses T-Cut to put a fine shine on shellac French polish (not all the time..but it’s one of his techniques). In fact it does work very well if you’ve painted on Shellac (using a rubber on fretworked concertina ends is a problem... you end up with dragged shellac clogging the holes). Paint on the shellac. Leave it for 24hrs to harden, fine wire wool it to take out the brush marks, then T-Cut.
Further side note: when I asked Mark Lloyd-Adey (Mr concertina spares) how he finished his concertina ends he told me he dilutes shellac a bit and sprays it on with one of those little spray guns.
-
Further side note: when I asked Mark Lloyd-Adey (Mr concertina spares) how he finished his concertina ends he told me he dilutes shellac a bit and sprays it on with one of those little spray guns.
And another side note. My daughter tells me that sprayed shellac is the way to the ultimate in painted fingernails.
-
Further side note: when I asked Mark Lloyd-Adey (Mr concertina spares) how he finished his concertina ends he told me he dilutes shellac a bit and sprays it on with one of those little spray guns.
And another side note. My daughter tells me that sprayed shellac is the way to the ultimate in painted fingernails.
Do they have to mask off the rest of their arm?
-
Stew-Mac makes some wonderful graded polishing cloths:
https://www.stewmac.com/luthier-tools-and-supplies/supplies/sanding-and-polishing/sandpaper-and-finishing-papers/micro-mesh-finishing-pack.html (https://www.stewmac.com/luthier-tools-and-supplies/supplies/sanding-and-polishing/sandpaper-and-finishing-papers/micro-mesh-finishing-pack.html)
and touch up sticks:
https://www.stewmac.com/luthier-tools-and-supplies/supplies/sanding-and-polishing/micro-mesh-dual-angle-touch-up-sticks-set-of-4.html (https://www.stewmac.com/luthier-tools-and-supplies/supplies/sanding-and-polishing/micro-mesh-dual-angle-touch-up-sticks-set-of-4.html)
that start at 1500 grit and end at 12000 grit going through 8 or 9 steps. For small jobs it will take you from dull matt to glossy sheen in a matter of minutes.
Scott
-
I have had a bit of experience (failing) with celluloid on a paolo soprani.
I found the pattern was on the top layer, but colour lower, and have rubbed through the top patterned layer.
I used wet and dry.
I really failed by having the acetone water mix too strong, so the celluloid melted too quickly, was trying to lay a large area.
Could be repaired as i have spare celluloid, but have moved on to other projects.
-
Ahh what a timely thread!! I was just trying to figure out how to rejuvenate my latest project. The green/grey celluloid is very faded and oxidized. I have a ton of car polish from full cut to mirror polish. I'll do some experimenting today. I like the carnuba wax idea as a sealer too.
-
I use brasso too, yes the cloth will show some colour because it is a very fine abrasive. Celluloid faces with exposure to light and air and an abrasive polish removes a very fine surface layer which can reveal unfaded material with a brighter colour. It’s exactly the same principle as a cutting polish on car finish.
Good to know, was worried! Thanks Theo, and the rest of you!
-
I was watching a Youtube vid on restoring a vintage guitar and when it came to replacing the pickguard he discovered something interesting. The old stock of celluloid he had had the colour and pattern throughout, whereas new stock has a plain colour in the material and a printed pattern on the top surface. In the context of our old boxes, the original covering can be expected to respond well to abrading and polishing to remove years of degradation, but beware of any patches and repairs which may contain modern material!
Rob.
-
Not all old celluloid has colour all the way through. I’ve seen ref celluloid from the 60s that has a thin red pearloid layer over grey.
-
"Do they have to mask off the rest of their arm?"
No they buff their arms so they are shiny and smooth like a mannikin.