Aluminium (Aluminum) oxidation
« on: August 18, 2015, 04:41:15 PM »

Hi

I am restoring a Hohner Club IV with an aluminium bulkhead on the treble side, and it's covered in white oxidation. Lord knows where it was left (outside or in a river) but I've cleaned out insects etc and completely disassembled the keyboard mech. On the reed block side there was an all over leather gasket, gone brittle and useless, which I'll replace, once I've cleaned up the aluminium, which has a heavy white powdery oxidation on both sides (worse under the leather). Astonishingly the rest of the box is pretty much ok (it has screwed in reeds - it's going to sound fab).
I'm thinking steel or brass brush(es) on my Dremel, steel brushing, scraping or, at a pinch, Dremel sanding disk as long as I don't pit the aluminium. I've read about various solutions but as this is mounted in the wooden case (I don't think it'll come out without force/unsticking it) I can't put anything wet in there. Any tips on cleaning aluminium? For some reason this is the second box I've had recently with this problem (the last one was left too long in a damp cupboard, according to its owner - I laboriously scraped it clean).
Thanks for any tips.


Steve_freereeder

  • Content Manager
  • Hero Member
  • ***
  • Offline Offline
  • Posts: 7511
  • MAD is inevitable. Keep Calm and Carry On
    • Lizzie Dripping
Re: Aluminium (Aluminum) oxidation
« Reply #1 on: August 18, 2015, 05:40:24 PM »

Whichever method you use to clean off the oxidation, the crucial thing is not to make and indentations or undulations in the flat aluminium surface or the bulkhead/fondo thingy.

I assume that one surface of the aluminium is where the pallets will bed up against. Creating any undulations on that surface will potentially result in air leaks between the aluminium and the pallet facing. Even small leaks have a significant detrimental impact on the playing efficiency of the instrument.

It is perhaps less critical on the reed block side of the aluminium if you are going to replace the all-over leather gasket, but any significant deviation from an overall flat surface again runs the risk of air leaks at the base of the reed blocks.

I would not use a dremel tool for this job, but only a sheet of fine (400 - 600 grade) carborundum paper fixed (glue? double-sided adhesive tape?) to a flat piece of wood used like a sanding block. Work evenly over the entire surface of the the fondo thing trying diligently not to create any hollows or undulations.

If the old leather gasket is proving difficult to remove, try gently dampening it with warm water on a sponge, then scraping carefully with a wood or plastic implement like a kitchen spatula. Then use the carborundum paper as above to remove any glue residue and get a smooth flat surface.
Logged
Steve
Sheffield, UK.
www.lizziedripping.org.uk

Rog

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2525
  • Repair and tuning in Hants
Re: Aluminium (Aluminum) oxidation
« Reply #2 on: August 18, 2015, 06:36:00 PM »

Hi Steve, thanks for that valuable advice. I did think of making a flat sanding block but not too large and with a handle. Sounds like the right thing then. The PA I recently cleaned up had air leaking through the fondo and it took me a while to detect little lumps of oxidation that were lifting the pallets. Once I had cleaned this off the leaks went away.

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #3 on: August 19, 2015, 12:41:22 AM »

If I read aright Roger you can access both sides, if the pitting is too deep for the sanding block Steve suggests to clean out of the pits without taking a lot of meat off,  follow up with bit of a red or grey scotchbrite pad on the block, which ought to get the rest out. A clean over with degreaser and a coat of aerosol clear lacquer should seal the surface against a repeat.

While look is not an issue, the graining which scotchbrite applies if applied linearly is very good at disguising ali which has had the shine taken off it and if the pad is fitted to an orbital sander and gently applied (like blotting wet ink) produces a very attractive mottling which disguises slightly more ingrained corrosion. (It can round over edges as fast as sheet abrasives if you go at it like a melodeonist with an air leak BTW  ;) )

Other abrasive loaded nylon pads are of course available...........
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Rob2Hook

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2278
  • Castagnaris, Hohners & Baffetti
Re: Aluminium (Aluminum) oxidation
« Reply #4 on: August 19, 2015, 02:05:42 PM »

Sounds like you've sorted how to scrub off the corrosion, but there must be concerns about the finishing of it to prevent a recurrence of the problem long-term.  Aluminium will oxidise under suitable conditions, forming an even coating which protects the bulk material.  Anodizing is the best hard, even finish you can achieve, but you;d need to get the plate out of the box and into an acid bath to achieve this.  All other finishes need an etching primer to adhere to the ally.  There is a finish called Alocrom which is in effect an etching primer, but doesn't need overcoating.  It is used in aerospace applications and similar when anodising is not possible.

Rob.
Logged

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #5 on: August 20, 2015, 12:01:25 AM »

You might be just the man to know Rob

I understand Aluminium oxide to be transparent and fairly corrosion resistant, one reason why they used to aluminise telescope mirrors, is it the other metals alloyed into what we tend to think of as Aluminium sheet which oxidise into that awfull grey/white crud or another oxide of Ali ??
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Rob2Hook

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2278
  • Castagnaris, Hohners & Baffetti
Re: Aluminium (Aluminum) oxidation
« Reply #6 on: August 20, 2015, 01:32:48 AM »

I think it's just an unwanted oxide of the aluminium - the alloying metals seem to have little influence. 

I went to visit a friend in Hickling a couple of months ago.  Hadn't been up that way for many years and was fascinated to find roadsigns to "Broadlands" - Que?  It always comes as a surprise to go through every village of a two week river cruise in ten minutes in a car.  Incidentally, I believe she's tryng to get a session going in the village.

Rob.
Logged

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #7 on: August 20, 2015, 01:48:52 AM »

Thanks Rob, I'd often wondered.

Not sure about 'Broadlands' sign - these days probably yet another housing development  >:(

Know what you mean, although during grain / spud / beet / set aside harvest it can be marginally quicker by boat  ;)

I'm not overly well informed but there are monthly sessions in the Orchard Gardens in N Walsham and the White Horse at Neatishead, your friend is probably better informed......
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Rog

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2525
  • Repair and tuning in Hants
Re: Aluminium (Aluminum) oxidation
« Reply #8 on: August 21, 2015, 09:21:19 AM »

If I read aright Roger you can access both sides, if the pitting is too deep for the sanding block Steve suggests to clean out of the pits without taking a lot of meat off,  follow up with bit of a red or grey scotchbrite pad on the block, which ought to get the rest out. A clean over with degreaser and a coat of aerosol clear lacquer should seal the surface against a repeat.

While look is not an issue, the graining which scotchbrite applies if applied linearly is very good at disguising ali which has had the shine taken off it and if the pad is fitted to an orbital sander and gently applied (like blotting wet ink) produces a very attractive mottling which disguises slightly more ingrained corrosion. (It can round over edges as fast as sheet abrasives if you go at it like a melodeonist with an air leak BTW  ;) )

Other abrasive loaded nylon pads are of course available...........

Hi..I'll also give the scotchbrite pads a go.  I can get little scotchbrite wheels for the Dremel but they wear out quickly and are expensive.
What sort of lacquer? Just a clear metal laquer?

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #9 on: August 22, 2015, 01:34:32 AM »

Go very carefully with the Dremel Roger, despite their small size they can shift an awful lot of material very quickly with scotchbrite (which is bad enough flat on a block) and will round edges over.

The sort of aerosol laquer from an auto shop for finishing over a metallic paint job would be my choice (Acrylic now in the UK, cellulose was better) should do, if the metal is warm, degreased & dry it should stick, sometimes you get a little crazing but this is internal so shouldn't matter, don'y know if there is some sort of clear etch primer available as noted earkier, I've only come across coloured.
HTH & good luck
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Kimric Smythe

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 712
    • Smythe's Accordion Center
Re: Aluminium (Aluminum) oxidation
« Reply #10 on: August 23, 2015, 05:24:52 AM »

Believe the oxides are caused by acids/metal salts in the leather, and can happen pretty quickly depending on the type of leather used.
Logged
Smythe's Accordion Center
Pinole, California
Sales and repairs since 1997

Nick Collis Bird

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 3785
  • Been squeezing melodeons for over 48 years (badly)
Re: Aluminium (Aluminum) oxidation
« Reply #11 on: August 23, 2015, 07:35:02 AM »

You're so right Kimric.
Leather used should be acid free around Ph 7. For books we only use leather that has been P.I.R.A. (Printing industries research association ) tested. eg. Acid free. Handbag,gloves etc. don't need this longevity. Bellows do and so do books!!
   A classic example. In the 70's a customer came into the shop and insisted I bound his valuable 1st edition in the leather he had supplied. I didn't like this and told him the reason why. He still insisted.
Ten years later he returned  the book with the cover in pieces. I didn't gloat , we rebound it and we haven't seen him since.  " the customer is always wrong" I should have stuck to my guns in the first place.
 
Logged
Has anyone heard of the song. “ Broken Alarm-clock Blues” ? It starts   â€œI woke up this Afternoon”

Rog

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2525
  • Repair and tuning in Hants
Re: Aluminium (Aluminum) oxidation
« Reply #12 on: August 23, 2015, 08:52:12 AM »

Believe the oxides are caused by acids/metal salts in the leather, and can happen pretty quickly depending on the type of leather used.
That would explain why my chisels, wrapped in a piece of leather then forgotten for  few months, had corroded and, while not ruined completely, require a fair bit of tlc to get them back to usefulness.

blue eyed sailor

  • Melodeon renegade - partly reverted - Preciosa maniac
  • Respected Sage
  • ****
  • Offline Offline
  • Posts: 264
  • since folk process is running, take an active part
    • My Sound Cloud
Re: Aluminium (Aluminum) oxidation
« Reply #13 on: August 24, 2015, 08:26:49 AM »

Believe the oxides are caused by acids/metal salts in the leather, and can happen pretty quickly depending on the type of leather used.
That would explain why my chisels, wrapped in a piece of leather then forgotten for  few months, had corroded and, while not ruined completely, require a fair bit of tlc to get them back to usefulness.

How would you use chisels with a melodeon?? >:E
Logged
Hohners: 2x Preciosa Bb/Eb (tremolo / light swing) - Club IV Bb/Eb - Morino Club C/F
Presswood C/F - Pokerwork C - Verdi II (PA) - Lucia IV (PA) - Starlet (PA)

Weltmeister 509 G/C/F - Juwel (PA) -- Horch C/F (12 bass) -- Cantulia Bambi 26 (PA)
and: Castagnari Giordy G/C

be warned of my SC page, mainly concertina thus far

Nick Collis Bird

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 3785
  • Been squeezing melodeons for over 48 years (badly)
Re: Aluminium (Aluminum) oxidation
« Reply #14 on: August 24, 2015, 11:45:56 AM »

To gouge out a name for yourself one presumes  8)
Logged
Has anyone heard of the song. “ Broken Alarm-clock Blues” ? It starts   â€œI woke up this Afternoon”

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #15 on: August 24, 2015, 03:08:20 PM »


How would you use chisels with a melodeon?? >:E
[/quote]

Not sure but the banjo repair manuals all specify large mallets  >:E
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Nick Collis Bird

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 3785
  • Been squeezing melodeons for over 48 years (badly)
Re: Aluminium (Aluminum) oxidation
« Reply #16 on: August 24, 2015, 03:41:01 PM »

Typo there. Did you mean large pallets? >:E
Logged
Has anyone heard of the song. “ Broken Alarm-clock Blues” ? It starts   â€œI woke up this Afternoon”

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #17 on: August 25, 2015, 01:22:42 AM »

Nope, not Barclays Nick  ;)
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa

Rog

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 2525
  • Repair and tuning in Hants
Re: Aluminium (Aluminum) oxidation
« Reply #18 on: August 26, 2015, 03:31:43 PM »

Clean out slot for inlay &etc

Broadland Boy

  • Hero Member
  • *****
  • Offline Offline
  • Posts: 1243
  • Awful noises from Pokerwork, HA114G, BbEb Liliputs
Re: Aluminium (Aluminum) oxidation
« Reply #19 on: August 27, 2015, 01:24:30 AM »

I've never quite understood the habit of quality steel tools being supplied with leather or cloth holders (or the US supplier of 'plane socks') Roger, perhaps they think everyone has a climate and humidity controlled workshop.

My workshop is unheated and well ventilated (the upper storey of an 1874 railway signal box) better quality woodworking handtools are kept oiled in a locked chest but it has long been overflowed by lesser tools of intermittent use and garden tools both of which increasingly I protect against rust by a wipe over with rag and some linseed (boiled) which is pretty durable - the metalworking stuff gets treated to a wipe over with Ensis fluid and slightly more controlled accomodation.

Leather or cloth if not otherwise buffered from the atmosphere will just absorb and transfer the humidity but my biggest problem is a sharp temperature increase after a frost when every metal surface in contact with the air pours with condensation.

All other aspects being equal I suspect the recipients of 60-70 year old melodeons with plastic valves will not find the same rust issues that their leather clad predecessors have done.

Warning, rags saturated in oils can spontaneously combust, so do not take your eyes off them day or night.
(or keep them in an airtight tin), even worse, an apparently dead battery (esp the PP3) and steel wool chucked in the bin will have a nice fire going in no time, especially if fed withy oily rags or tissue  :o

As for storage of small ferrous parts, for durability, stackability & airtightness there is little to beat the rectangular 2oz / 50g tobacco tin, some originally stocked by grandfather have kept their contents bright and shiny since the 1930's.
Logged
Richard A
Venit ventus contrarius ventus egrediente,
Omnes prope quid ventum est circa
Pages: [1] 2   Go Up
 


Melodeon.net - (c) Theo Gibb; Clive Williams 2010. The access and use of this website and forum featuring these terms and conditions constitutes your acceptance of these terms and conditions.
SimplePortal 2.3.5 © 2008-2012, SimplePortal